CS85
This board was developed to be a high temperature replacement for asbestos Transite. It offers our highest strength and electrical resistance combined with minimal shrinkage for applications up to and exceeding 1800°F. Potential applications include platen press insulation, foundry core and blow plates, induction furnace casing, electrical resistance insulation, hot glass handling and numerous others.
Properties
| Dimensions |
| Available Thicknesses |
¼-3" |
| Sheet Sizes |
4' x 8' |
| Density |
| pcf |
85 |
| kg/cm3 m3 |
1362 |
| Modulus of Rupture |
| psi |
3000 |
| kg/cm² |
210 |
| Compressive Strength |
| Ultimate load: psi |
10300 |
| Ultimate load: kg/cm² |
724 |
| @ 5% Deformation: psi |
6400 |
| @ 5% Deformation: kg/cm² |
450 |
| Moisture |
| Normal % of dry wt |
1.0 |
| Thermal Conductivity (Mean Temperature, Btu-in/ft2, hr, °F) |
| 400°F |
2.13 |
| 800°F |
1.94 |
| 1000°F |
2.01 |
| Thermal Conductivity (Mean Temperature, W/m°K) |
| 204°C |
0.31 |
| 427°C |
0.28 |
| 538°C |
0.29 |
| Shrinkage%: 24 hrs @ 1600°F |
| Length/width |
0.24 |
| Thickness |
2.0 |
| Electrical |
| Arc Resistance, Seconds ASTM D 495 |
304 |
| Volume Resistivity, ohm-cm ASTM D 257 |
4.52 x1012 |
| Dielectric Strength, v/mil ASTM D495 |
61 |
| Screw Holding Strength @ 7/8" penetration |
| lbs |
895 |
| kg |
397 |
The physical and chemical properties of BNZ's materials represent values obtained in accordance with accepted test methods and are subject to normal manufacturing variations. They are supplied as a technical service and are subject to change without notice. Results should not be used for specification purposes.
|
|  |
 |
|
|
 |